Effect of circulating elements on the dynamic reduction swelling behaviour of olivine and acid Iron ore pellets under simulated blast furnace shaft conditions

Iljana, Mikko; Mattila, Olli; Alatarvas, Tuomas; Kurikkala, Jari; Paananen, Timo; Fabritius, Timo (2013-01-01)

 
Avaa tiedosto
nbnfi-fe202101202245.pdf (1.563Mt)
nbnfi-fe202101202245_meta.xml (39.99Kt)
nbnfi-fe202101202245_solr.xml (32.31Kt)
Lataukset: 

URL:
https://doi.org/10.2355/isijinternational.53.419

Iljana, Mikko
Mattila, Olli
Alatarvas, Tuomas
Kurikkala, Jari
Paananen, Timo
Fabritius, Timo
Iron and Steel Institute of Japan
01.01.2013

Iljana, M., Mattila, O., Alatarvas, T., Kurikkala, J., Paananen, T., Fabritius, T. (2013) Effect of Circulating Elements on the Dynamic Reduction Swelling Behaviour of Olivine and Acid Iron Ore Pellets under Simulated Blast Furnace Shaft Conditions. ISIJ International, 53 (3), 419-426. https://doi.org/10.2355/isijinternational.53.419

https://rightsstatements.org/vocab/InC/1.0/
© 2013 by The Iron and Steel Institute of Japan.
https://rightsstatements.org/vocab/InC/1.0/
doi:https://doi.org/10.2355/isijinternational.53.419
Näytä kaikki kuvailutiedot
Julkaisun pysyvä osoite on
https://urn.fi/URN:NBN:fi-fe202101202245
Tiivistelmä

Abstract

Sulphur and alkalis in the blast furnace gas have been associated affecting the reduction swelling behaviour of iron ore pellets. A tube furnace was used in this study to examine the dynamic reduction swelling behaviour of olivine and acid pellets in CO–CO₂–N₂ atmosphere with sulphur and potassium in gaseous phases up to 1100°C simulating the conditions in the blast furnace shaft.

No abnormal swelling was detected in sulphur or potassium containing CO–CO₂–N₂ atmospheres during dynamic reduction. Instead, sulphur in the reducing atmosphere was associated with pellet contraction and FeO–FeS melt formation which became more dominant with increasing sulphur partial pressures. In the extreme case, having a maximum of 1.0 vol-% S₂ gas in the reducing atmosphere, the reduction reaction of wüstite to metallic iron was hindered. The formation of FeO–FeS liquid phase extends the cohesive zone towards the blast furnace top and lower temperatures and decreases the gas permeability. Furthermore, large amounts of potassium in the reducing atmosphere (max. 0.03 vol-%) led to swelling and cracking in the olivine pellets still remaining in the range of normal swelling.

Kokoelmat
  • Avoin saatavuus [38841]
oulurepo@oulu.fiOulun yliopiston kirjastoOuluCRISLaturiMuuntaja
SaavutettavuusselosteTietosuojailmoitusYlläpidon kirjautuminen
 

Selaa kokoelmaa

NimekkeetTekijätJulkaisuajatAsiasanatUusimmatSivukartta

Omat tiedot

Kirjaudu sisäänRekisteröidy
oulurepo@oulu.fiOulun yliopiston kirjastoOuluCRISLaturiMuuntaja
SaavutettavuusselosteTietosuojailmoitusYlläpidon kirjautuminen